Time:2012.10.11News SourcesViews:
The solid wood floor tiles flooring industry development in China earlier a traditional product, made the product directly from natural wood machining, and thus has a natural beauty, cool, non-toxic, foot feeling good and noble characteristics by the majority of consumers of all ages, and has been one of the leading products in the wood floor. Especially in recent years, with the increasing people's living standards, indoor decoration industry is booming, is also gradually expanding the production and sales volume of the solid wood flooring, solid wood flooring species from the original oak, birch, ash mainly the development of dozens of species mainly imported species, and several other species, able to satisfy the needs of the society and people's lives. Solid wood flooring, however, also appeared in the course of a lot of quality problems, specifically manifested in the following aspects:
① distortion; ② floor between the gap is too large; ③ arch; The ④ floor between the height difference is too large; ⑤ floor in corrugated; ③ floor cracks; ⑤ paint paint peeling, crack, wrinkle; ③ floor discoloration.
Reason from the big perspective pavement quality, the quality of the floor and use improper three aspects due to specific reasons are analyzed as follows:
① cause the floor distorted main reasons: a. Timber production floor material is not suitable; b. Process derived improper; The moisture content of the floor to control uneven or floor moisture content is not suitable for the use of environmental requirements.
The ② caused by a too large gap between the floor are: a. The floor of the moisture content is too large; b. Indoor environment is too dry; C. The quality of laying on the floor, causing the floor to produce mobile.
The ③ floor arched reasons: a. Pavement when the the reserved gap between the floor and wall base is not enough; b. Reserve gap is not enough room to room without making the bridge or bridge; When laying floor's moisture content is too low; d. Room due to water leaks, the floor soaked by water; e. The ground is wet or humid keel timber.
④ floor height difference is too big for two reasons: a. Uneven ground; b. Keel laying uneven; C. Floor thickness deviation; d. Floor deformation; e. Flooring tongue and groove processing does not match.
⑤ floor corrugated reasons: a. Cement laying on the floor, uneven ground, the keel the moisture content is too large; b. Dry indoor environment; Floor moisture content is too high; d. Indoor ambient humidity is too low floor moisture content.
The ③ floor cracks reasons: a. Timber performance is not suitable for the production of wood flooring; b. The high moisture content of the wood flooring, dry, low humidity and indoor environment.
③ paint film peeling, cracking and wrinkling of reasons: a. Paint performance is not suitable for the flooring species, resulting in film and adhesion properties of wood can not meet the requirements, there spalling; The toughness of the paint film can not meet the the the wood naturally wet rose shrinkage of changes to enable the film to crack wrinkling; C. Caused by poor adhesion of paint topcoat and primer topcoat spalling; d. The paint flaking paint process unscientific, crack, wrinkle; e Film wrinkling peeling; f floor moisture content is too high. Floor moisture content is too low to cause cracking or flaking of the paint film; Zhao. Harsh indoor environments, such as indoor environment is too dry or too wet will result in film damage.
The ③ floor discoloration mainly due to: a. The discolored wood itself generated by the impact of the external environment, such as sunlight, indoor air environment; The paint changes generated by the impact of the external environment; C. The chemical reaction between the paint and the timber due to a change.
To avoid the floor quality problems during use, you must do the following aspects:
1. Laying on the floor, floor, wall, wall base to ensure dry.
2. The ground should be leveled.
3. Keel and use the liner to be dried, the moisture content of not more than the local equilibrium moisture content.
4 keel plane to be smooth.
5. The best ground-laying of the floor before laying a layer of plastic film.
6. The moisture content of the wood floor to ensure that the standard range, do not exceed the local equilibrium moisture content.
7. For manufacturers in terms of scientific flooring species, not suitable to do the floor of the species, and should never be used.
8. Wood species different physical, chemical and mechanical properties are different, so the factory in the selection of paint should be tested. Confirm the adaptability of the paint on the wood species, the scientific selection of paint to paint meet the performance.
9. Between the floor and wall base, wood flooring, doorways, etc. should be reserved according to the room size sufficient expansion joints.
10. In the process of laying the floor, try not to use water-soluble adhesive to avoid due to the floor to absorb moisture causing swelling, deformation;
11 is sure to hit the keel with cement fixed keel.
12. Indoor environment not too dry, nor too wet, especially in the north in winter, indoor humidity keep prevent chapped, deformation of the wood flooring.
13. Try not to use when cleaning the floor, cleaning the floor with dripping Tuoshi.